1.high-temperature mullite insulation bricks
2.high-purity hot-mullite c
3.energy-efficient material
Insulating firebricks HS
High-temperature mullite insulation bricks
High-temperature mullite insulation bricks are
Max operate temperature of test ite items
Designtion |
HSMJ20 |
HSMJ23 |
HSMJ26 |
HSMJ28 |
HSMJ30 |
HSMJ32 |
||
1300 |
1350 |
1430 |
1540 |
1650 |
1760 |
|||
Bulk density(g/cm3) |
0.5-1.0 |
0.5-1.0 |
0.8-1.0 |
0.9-1.0 |
0.9-1.2 |
1.2-1.25 |
||
Cold crushing strength(Mpa) |
0.9-1.2 |
1.2-3 |
3.5-4 |
4-4.5 |
4.5-5 |
5-5.5 |
||
Degree of room temperature flexral(Mpa) |
0.7-1.0 |
1.0-1.3 |
1.5-1.8 |
1.9-2.0 |
2.0-2.1 |
2.1-2.2 |
||
Permanent linear change(%) |
-0.98 1200*24h |
-0.5 1300*24h |
-0.5 1400*24h |
-0.5 1500*24h |
-0.5 1510*24h |
-0.5 1600 *24h |
||
Load softening starting point(.C) |
1100 |
1250 |
1350 |
1450 |
1500 |
1600 |
||
Thermal conductivity W/(m.k)350C±10C |
0.12 |
0.15 |
0.25 |
0.32 |
0.38 |
0.47 |
||
Thermal shock resistance(time)1000.C air cooled |
≥20 |
≥20 |
≥20 |
≥20 |
≥20 |
≥20 |
||
Chemical compostion |
Al2O3(%) |
≥45 |
≥50 |
≥60 |
≥70 |
≥75 |
≥80 |
|
Fe2O3 |
≤1.0 |
≤1.0 |
≤0.8 |
≤0.7 |
≤0.6 |
≤0.5 |
||
SiO2 |
55 |
40 |
35 |
35 |
18 |
16 |
||
CaO |
1.8 |
1.7 |
1.7 |
1.4 |
1.2 |
1.0 |
||
SiC |
- |
- |
- |
- |
- |
- |
||
ZrO |
- |
- |
- |
- |
- |
- |
||
MgO |
0.2 |
0.1 |
0.1 |
0.1 |
0.1 |
0.1 |